The effect of magnetite as a magnetic seed on the flotation separation of fine hematite and quartz was studied by reverse micro-flotation and sedimentation. The results demonstrate that fine magnetite could selectively report to the pulp product with hematite particles, forming aggregates that avoided attachment to quartz particle surfaces.
1. Introduction. As the principal input material in industries of steelmaking, coating and durable pigments, hematite is an oxidized iron mineral ore with a formula of Fe 2 O 3 (Pauliuk, Milford, Müller, & Allwood, 2013).The major gangue mineral is quartz in oxidized iron ore, and reverse flotation is the most common method to beneficiate iron …
Hematite and Quartz Minerals for Flotation ", 4 th UMaT Bien nial International Minin g and Mineral Conference, pp. MR 67-73. Abstract . Monazite is a principal rare earth (RE) ...
The flotation results of single minerals revealed that the reagents scheme of CMCS/DDA could be used in the reverse flotation of quartz from hematite. The flotation tests of mixed hematite and quartz in the mass ratio of 4:1 were carried out in the presence of 60 mg/L collector and 12 mg/L depressant at pH 8.
In the reverse cationic flotation process of hematite and quartz, the most commonly used cationic collectors are amine collectors, such as dodecylamine (DDA) and ether amine, etc [7], [14]. In this process, the quartz needs to be floated out and the target mineral hematite is suppressed. Usually, under the reaction of the cationic collector DDA …
In this study, the flotation system with hematite, quartz and dodecylamine (DDA) as collector was used as an example to quantify the types and densities of active sites on the surfaces of hematite ...
Flotation of mixed minerals (hematite and quartz mixture in various ratios) indicated that LGB could enhance separation efficiency (hematite recovery > 88%). …
Therefore, the pre-adsorption of PASP on the hematite surface hinders the adsorption of the collector DDA. Therefore, the depressant PASP selectively inhibits hematite in the reverse flotation of hematite from quartz. 4. Conclusions. Hematite and quartz have excellent floatability and were difficult to be separated by flotation using …
DOI: 10.1016/j.apsusc.2023.157064 Corpus ID: 257647038; Investigation into starch adsorption on hematite and quartz in flotation: Role of starch molecular structure @article{Yang2023InvestigationIS, title={Investigation into starch adsorption on hematite and quartz in flotation: Role of starch molecular structure}, author={Siyuan Yang and …
Currently beneficiation of hematite ores is conducted using either direct flotation (hematite flotation) or indirect flotation (quartz flotation) tech-niques depending upon the nature …
The mineral mixture test was carried out in the mass ratio of 75:25 "hematite: quartz". The batch flotation test was conducted using a 1 L Denver D12 laboratory flotation cell. The solid ...
The tests were divided in two categories: single mineral flotation and a 1:1 mix of hematite–quartz flotation. The samples were in the 100×74-μm size range. In carrying out the experiments, 1.0 g (for single mineral flotation) or 0.7 g of each mineral (for mixed sample) was first conditioned for 10 min with 135 ml of cellular suspension of ...
Flotation of mixed minerals (hematite and quartz mixture in various ratios) indicated that LGB could enhance separation efficiency (hematite recovery > 88%). Outcomes of the surface wettability indicated that even in the presence of the collector (dodecylamine), LBG decreased the hematite work of adhesion and had a slight effect on quartz.
Flotation results showed that the success of anionic reverse flotation of hematite was inseparable from the activation of quartz by Ca2+. In addition, the use of …
The flotation separation of hematite and quartz usually adopts a reverse flotation process, that is, hematite is depressed to collect quartz [ 4 ]. Therefore, …
Selective aggregation of hematite with magnetite enhanced selectivity of flotation separation of fine hematite from quartz. Fine magnetite served as a …
The cation reverse flotation is a widely used method in improving the grade of iron ore concentrate, but hematite depressant is the key. In this work, the flotation behavior of hematite and quartz using the complex of Fe(III) and xanthan gum (Fe(III)-XG) as depressant was investigated via micro-flotation tests.
The traditional hematite depressant starch has the disadvantages of poor solubility and high viscosity. In this study, a novel hematite depressant, pullulan, with better performance and flotation effect than starch was found. The structure, molecular weight and viscosity of pullulan were determined for its characterization. The results of flotation …
The flotation performances of muscovite and quartz had been studied using DDA, NaOL and mixed NaOL/DDA with various molar ratios. Fig. 1 shows flotation recoveries of muscovite and quartz as a function of pH in the presence of different collectors. It can be seen that with an increase of pH from 2 to 11, the recovery of …
The results also show that quartz flotation recovery decreased steadily from pH 3 to 11, which is consistent with the results obtained from the electrokinetic measurements (Section 3.3.3). Floatability curves as a function of pH for monazite, hematite, and quartz in the presence of 1000 g/t AH are presented in Fig. 8. The …
flotation (hematite flotation) or indirect flotation (quartz flotation) tech-niques depending upon the nature of the available ore bodies. In direct flota-tion, iron bearing mineral, mostly hematite, is floated using oleate as collec-tor leaving siliceous gangue, usually quartz, in the tailings. Kick et al. [1]
In this study, an asynchronous flocculation method was explored in the flotation separation of mixtures of ultra-fine hematite (d 50 = 7.2 µm) and ultra-fine quartz (d 50 = 1.6 µm) using polyethylene oxide (PEO) and starch as the flocculant of quartz and hematite, respectively. Dodecylamine acetate was used as a collector for quartz in the ...
The physical and chemical properties of feldspar and quartz are highly similar, thus they cannot be easily separated effectively. In this work, the flotation separation of feldspar from quartz using sodium fluosilicate (Na 2 SiF 6; SF) as a selective depressant was investigated.Moreover, the influence mechanism of SF on the selective …
Native starches and their phosphates with various molecular structures was introduced as the depressant to realize the flotation of quartz from hematite in this study. The present starch phosphates (WSP, NSP, GSP) were modified by the reaction between phosphate and three different corn starches (WS, NS, G50). The synthesis and …
The optimum flotation pH for hematite and quartz was firstly determined. Flotation tests for hematite and quartz were carried out at a dodecylamine dosage of 30 mg/L without the addition of starch. Fig. 5 shows that the flotation recoveries of both minerals first increased and then decreased over pH. The maximum recoveries of …
Cationic/Anionic Collectors in Quartz–Hematite Flotation System, Mineral Processing and Extractive. Metallurgy Review: An International Journal, 35:2, 117-125, DOI: 10.1080/08827508.2012.723649.
The challenge of monazite flotation selectivity from hematite–quartz mixtures was aggravated by quartz surface activation by soluble cations from hematite and monazite resulting in the entrained recovery of quartz. In order to depress hematite and quartz, sodium silicate and starch were tested. Both depressants produced desirable …
Flotation of the synthetic mixture of hematite: quartz (1:1), with Aliquat-336 as the quartz collector and starch as the hematite depressant, has resulted in an iron concentrate of 63–65% Fe ...
It is essential to investigate flotation behavior of siderite-hematite-quartz for processing those iron ores. To this end, flotation of the three pure minerals was carried out in sodium oleate system in this work. Flotation theory mainly consists of flotation solution chemistry, interfacial chemistry and flotation kinetics [18].
The flotation recoveries of the hematite and quartz were explored as a function of Flotigam®EDA concentration in the absence and presence of 100 mg/L TA (Fig. 3). It was shown that the quartz recovery in the whole range of Flotigam®EDA concentration was higher than the hematite.
The cation reverse flotation is a widely used method in improving the grade of iron ore concentrate, but hematite depressant is the key. In this work, the flotation behavior of hematite and quartz using the complex of Fe(III) and xanthan gum (Fe(III)-XG) as depressant was investigated via micro-flotation tests.
Flotation results with both quartz and hematite indicate an increased adsorption of cationic collector in the presence of anionic collector apart from its …
1. Introduction. In Brazil, reverse cationic flotation has been the most commonly used route for the concentration of itabirite [[1], [2], [3]].In the process, quartz is recovered in the flotation froth in the presence of etheramine (R O (CH 2) 3 NH 2), and the iron mineral content is usually depressed by corn starch, a mixture composed of …
The selectivity window between quartz and hematite flotation using amide-amine was higher at pH 10.5 (approximately 80% for 5 mg/L). Therefore, the use of …
DOI: 10.1016/J.MINPRO.2016.11.012 Corpus ID: 99083826; A study of flotation characteristics of monazite, hematite, and quartz using anionic collectors @article{AbakaWood2017ASO, title={A study of flotation characteristics of monazite, hematite, and quartz using anionic collectors}, author={George Blankson Abaka-Wood …